Not aimed at anyone directly but getting your paint layers really thin, especially undercoats helps massively when sharpening up the look of your models. From a lot of years experience painting this might help a few 
Undercoating
- USE A SPRAY! Undercoatign by hand will be so much thicker
- I know this is massivly common sense but a really long shake of any undercoat paints helps get a very smooth thin layer first time, 30 seconds minumum, longer if youve not used the undercoat in a while.
- Also starting and stopping your undercoat sprays is adding more layers of undercoat than you need, try be continuous with your flow of spray if at all possible.
- If you find that pressing down the top of the undercoat makes your finger freeze up, a rubbber thimble or a chopped off bit from a marigold helps youkeep it pressed for longer. (Tip from an old work colleague)
- I found that most of the time If I was undercoating I'd try and get it as thin as possible and only use one coat. Any thin areas left after the sparying can be touched up with a slightly waterde down paint of the same colour.
- Undercoating/leaving to dry in a really cold area will sometimes lead to graining on your paint. Dont undercoat when its -2 outside!
If I think of any more I'll add in on

Undercoating
- USE A SPRAY! Undercoatign by hand will be so much thicker
- I know this is massivly common sense but a really long shake of any undercoat paints helps get a very smooth thin layer first time, 30 seconds minumum, longer if youve not used the undercoat in a while.
- Also starting and stopping your undercoat sprays is adding more layers of undercoat than you need, try be continuous with your flow of spray if at all possible.
- If you find that pressing down the top of the undercoat makes your finger freeze up, a rubbber thimble or a chopped off bit from a marigold helps youkeep it pressed for longer. (Tip from an old work colleague)
- I found that most of the time If I was undercoating I'd try and get it as thin as possible and only use one coat. Any thin areas left after the sparying can be touched up with a slightly waterde down paint of the same colour.
- Undercoating/leaving to dry in a really cold area will sometimes lead to graining on your paint. Dont undercoat when its -2 outside!