Galvanic corrosion/rust ?

Associate
Joined
10 Apr 2014
Posts
789
Location
Hampshire
I know what the term galvanic corrosion means, when two different metals are used in the same cooling loop it causes corrosion.

I havent experianced this before because the loop it has happened in, is my first build. So technically i have experianced it, if this is it.

The water has been in there for 2/3 years and has had 2 mayhems silver kill coils in the res and two different filters.

evoLJ12.jpg


If you look closely at the filter before the flow indicator you can see dark specs, im guessing those are bits of metal left over from manufacturing that have been caught.

VIwXdR7.jpg

BOITeJr.jpg


I think there is a bit of rust on the inside of one of my fittings aswell but, looking at these pictures, can anyone tell me wether this is corrosion or rust?

Im guessing that if it is either one of them then cleaning the block isnt an option and I should replace it and the fittings aswell (also an excuse to not address the build up around the gaskets)

What is it based on the pictures ?
 
Yup.

Better yet, remove the two silver coils and make sure the loop has inhibitor and biocide, or use a premix with both. Problem solved.

I have bought some mayhems x1 clear and some new tubing. I cleaned the gpu block and didnt get all of it off but most of it, maybe 95% lol. If i add the pre mix will the state of the loop stay as it is, will there be a chance of anymore corrosion?
 
Make sure you remove the silver coils. They will cause issues with nickle plated blocks as you have seen.
Clean up as best you can (toothpaste is good for this) and flush thoroughly to be sure the loop is clean.

Make sure you really flush the rad(s) completely. This is worth saying twice.

The x1 claims to protect against corrosion, scale and biological fouling of the loop so once everything is clean you should be set.

With the X1 i imagine everything should be good for a year or more depending on temps and sunlight etc.

I have some mayhems blitz part 2 already mixed, it has been in a bottle in my room for about a year or so, i was planning on using that before using the x1, the bottle of the part 2 itself says to run it in the loop for 12 to 24 hours so i imagine that is enough for the cleaning. I already used my dedicated block cleaning solution(colgate whitening).
 
Yup.

Better yet, remove the two silver coils and make sure the loop has inhibitor and biocide, or use a premix with both. Problem solved.

Got the block “cleaned” and flushed the loop with part 2, also rinsed with mayhems h20 and after putting it back together it didnt look like anything was actually cleaned lol. The gunk is gone from the gasket atleast. Now I have the x1 clear in there, maybe it will keep it at the condition that its in and not make it any worse.
 