Galvanic Corrosion

Associate
Joined
25 Feb 2011
Posts
415
Location
North East
I'm just about to start a new computer build and just want to check a question about waster cooling before I start anything because I'm a newbie to it. If I want to build my own reservoir out of some stainless or aluminium pipe to sit outside the case, cpu cooler and rad have copper in, so am I right in thinking as long as I don't ground the res to the case I shouldn't have any problems as there wouldn't be a complete circuit?
 
It is generally considered a bad idea to mix metals in a water cooled system. There are heaps of thread over at XS that flog that particular horse to death.
 
Make the res out of perspex, then sleeve it in aluminium...

That way the loop itself only has one metal actually in contact with the liquid :)

That said, how about the fixings? they're not copper are they..?
 
Mixed metal loop just need the right coolant.
Unless its has dis-simular metals in direct contact like the old swiftech GTX.
Thats just asking for trouble.

Building your own is imho not really for a noobie, not sure why you want a 'pipe' reservoir
But if you have the skills there are a few here that have, and will happily offer advice.
Money puzzles, project HUSH is a good place to start.

Pictures many help with bubo questions - all are external RAD's which it what I think you ment, so....

Are you looking to do something like this (this has a mixed metal passive loop)

lian-li-a01-02.jpg


or this (home made rad box for a AV system - fan assisted all copper/brass)

IMG_1994.jpg


or this (modified commercial passive water loop - mine and mixed metal)

workstation.jpg


or this (commercial passive free standing rad - mixed metal)

HTCS1a.jpg


or this (home made, radient panel rad - mine all copper/brass)

toweroffour.jpg
 
Last edited:
Thanks for the replies, I was thinking of something similar to the XSPC passive radiator. I can get some large bore pipe that would be wide enough for free and just seal the ends with some spare sheet and then cover the outside in corrugated sheet. I wanted it outside the box just for looks, there will also be a normal radiator in the loop to do most of the cooling.
To stop corrosion is there any special paints/coatings that could be used?
 
You mean "XSPC 150/250mm Passive Aluminium Reservoir"
If you could get the tube anodized that would help
Or an marine grade paint for the inside would also stop the collant 'touching' the metal.
But will reduce heat transfer.

your biggest issue if fitting barbs
A 2 or 3mm metal plate can be tapped with a G1/4 thread
Or you could just weld them on.
 
Yes, I meant reservoir but for some reason radiator poped into my head.
Welding is no problem so I would go that way, do you have a build log for the radient panel rad you made? I might just go down the copper pipe route if it is safer!
 
I ran a mixed system copper blocks with Aluminium Radiator and Reservoir for years without issue. Used distilled (not deionised)water with anti corrosion additive. The Aluminium parts were anodized though and I think this was key. I got a scratch in the finish after sometime and at that particular spot corrosion started to happen fairly quickly. So I would not recommend bare Aluminium.
 
As shadowscotland says there is no problem with mixed metals in loops, You just need a corrosion inhibitor in your coolant.
Antifreeze will serve this purpose very well. 10 - 15 % mix is plenty

My sons system we made has a cast iron / aluminium pump, aluminium radiator, copper blocks and pipes.
This has been running for the past 4-5 years with out a hitch
 