Just waiting on my Caselabs THW10 which will be sent out for delivery on January 6th, I already have all my watercooling parts but need help with one last thing Corrosion.
I have been reading that the EK nickel blocks that I have are no way suitable with a silver coil and will cause galvanic corrosion over time, I will be using Mayhems ultra pure H20 with the Mayhems blue dye I have also ordered Mayhems biocide extreme.
What I want to know is will I be fine with just the biocide extreme or do I need something else instead of the silver coil that I cant use? I really don't want to use premixed coolants as they tend to gunk up your blocks, thanks SpringY1989.
 
personally I just go with the mayhems pre-mix or concentrate. Everything you need in the right proprtions.
 
I ran Mayhems Ultra H20 with their blue dye and a few drops of biocide extreme for nearly two years before I changed the coolant.

worked fine. no gunk in the blocks but that Mayhems blue dye is a pig to clean out and stains everything.

Of course they make a clening kit for that.
 
I ran Mayhems Ultra H20 with their blue dye and a few drops of biocide extreme for nearly two years before I changed the coolant.

worked fine. no gunk in the blocks but that Mayhems blue dye is a pig to clean out and stains everything.

Of course they make a clening kit for that.
Awesome pal I can cope with cleaning no problem thanks for the update.
 
I'm sure it would be fine as that's the whole point on electroplating the block with nickel is that it doesn't react but just ditch the silver coil.

I ran a distilled water loop with just a couple of drops of PT nuke, basically the same as the biocide you have brought for 2 years with no maintenance once and it had no problems.
 
I'm sure it would be fine as that's the whole point on electroplating the block with nickel is that it doesn't react but just ditch the silver coil.

I ran a distilled water loop with just a couple of drops of PT nuke, basically the same as the biocide you have brought for 2 years with no maintenance once and it had no problems.
Thanks mate for the update :D
 