Heh well my previous tubing was XSPC High Flex. When I did my annual maintenance I switched to Primochill Advanced.
Like I said, in my case a small amount of gunk was stuck between the fins on the block. Nowhere near as bad as OP. This was a dark/red colour rather than white though, so guess it could be plastisiser. Water temps didn't go over 40oC throughout though, as far as I am aware. I had read higher temps exacerbate the situation, wonder what OPs temps were?
Hopefully next time I won't notice anything at all.. time will tell!
Like I said, in my case a small amount of gunk was stuck between the fins on the block. Nowhere near as bad as OP. This was a dark/red colour rather than white though, so guess it could be plastisiser. Water temps didn't go over 40oC throughout though, as far as I am aware. I had read higher temps exacerbate the situation, wonder what OPs temps were?